If it is assumed that, for steel alloys, the average cooling rate of the heat-affected zone in the vicinity of a weld is 10 oC/s, compare the microstructure and associated properties that will result for 1080p (eutectoid) in its HAZ (Heat Affected Zone)

answer
Answers: 3

Other questions on the subject: Physics

image
Physics, 22.06.2019 02:30, chycooper101
Aforce of 9.00 newtons acts at an angle of 19.0 to the horizontal. what is its component in the horizontal direction?
Answers: 2
image
Physics, 22.06.2019 14:30, zuleromanos
70 give a real life example showing how sensory neurons work with the motor neurons
Answers: 2
image
Physics, 22.06.2019 16:40, dylan6981
The astronauts on the space shuttle flights experienced an acceleration of 29 m/s2 (about 3 "g's") during lift-off. what upward force must the astronaut's seat apply to the astronaut in order to cause this acceleration? assume the astronaut's mass is 70 kg, and compute this force when the acceleration is near the earth's surface so their weight equals latex: mg m g .
Answers: 3
image
Physics, 22.06.2019 21:00, cici65360
What do the atoms of elements in the same group have in common? a. they have the same atomic numbers. b. they have the same average atomic masses. c. they have the same number of electron shells. d. they have the same number of electrons in their outermost shells.
Answers: 1
Do you know the correct answer?
If it is assumed that, for steel alloys, the average cooling rate of the heat-affected zone in the v...

Questions in other subjects: